Emulsion buffer mitigates screen-printing degradation in copper-plated HJT cells

A 4.7% emulsion coverage pattern limited minority-carrier lifetime degradation to 0.41% after 10,000 printing cycles, researchers report.

Maya LindqvistNovember 15, 20265 min read2 views

A conceptual close-up shows a fine metal screen mesh and patterned blue emulsion layer held above a solar cell wafer in a clean research setting.

Researchers in China have investigated how photoresist screen printing damages copper-plated silicon heterojunction (HJT) solar cells and have proposed a modified screen design to limit the effect. The work focuses on a metallization route that could reduce metallization costs and reliance on silver, but the printing step itself can harm the cell’s sensitive passivating contacts.

Screen printing is widely used to form metal contacts on solar cells. In copper-plated HJT devices, however, the process is used to apply photoresist across the full wafer area. Mechanical pressure and thermal treatment during printing can damage passivating contact structures, raising recombination losses and lowering conversion efficiency. Understanding the degradation mechanism is therefore important for optimizing metallization without sacrificing cell performance.

Why photoresist printing differs

Corresponding author Lang Zhou explained that photoresist printing differs fundamentally from conventional silver-paste screen printing. In silver printing, screen openings account for only 2–5% of the total area, and an emulsion layer covers the rest of the surface, preventing direct contact between the mesh and the wafer. Full-area photoresist coating typically uses a screen without emulsion coverage so that resist can be deposited uniformly across the wafer. As a result, the mesh comes into direct and extensive contact with the wafer during every printing cycle.

Measured losses

Previous investigations cited by the researchers found that conversion efficiency fell from 26.2% to 25.7% over 15,000 consecutive printing cycles in commercial solar cell production. The losses were mainly linked to reductions in open-circuit voltage and fill factor, while short-circuit current density and electrical resistance remained largely unchanged. Minority carrier lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 printing cycles.

Using three-dimensional confocal microscopy, the team identified progressive wear of the screen mesh knuckles as the main cause. As the knuckles wore down, their contact area with the wafer increased, placing greater mechanical stress on the underlying passivation layers. Scanning electron microscopy showed no visible surface scratches, but photoluminescence measurements confirmed higher recombination losses, suggesting damage to the amorphous silicon/crystalline silicon interface.

Emulsion buffer trade-off

To reduce that damage, the researchers developed an emulsion buffer layer intended to prevent direct contact between the screen mesh and the wafer. They evaluated six patterns with emulsion coverage ratios from 2.9% to 16.6%. The results revealed a trade-off: higher emulsion coverage reduced mechanical damage but impaired photoresist coating uniformity and ink distribution.

A coverage ratio of 4.7% provided the best balance, limiting minority carrier lifetime degradation to 0.41% after 10,000 printing cycles while maintaining relatively good coating uniformity. The researchers attributed the improvement to the emulsion layer blocking direct mesh-to-wafer contact and thereby reducing cumulative mechanical damage to the passivation layers.

Zhou said the findings indicate that a relatively simple change to screen design can substantially mitigate printing-induced degradation and offer a practical approach to improving the manufacturing reliability of copper-plated HJT cells. The results were published in Solar Energy in the paper “Screen-printing photoresist induced efficiency degradation and mitigation in Cu-plated SHJ solar cells.”

The work arrives amid growing interest in copper metallization as an alternative to silver contacts in HJT solar cells. In April 2026, researchers at China’s Nankai University reported a silver-free HJT cell with 25.2% efficiency using plasma-induced interface engineering and copper electroplating, addressing adhesion, contact resistance and stability at the ITO interface. Separately, scientists at Germany’s Forschungszentrum Jülich achieved 23.08% efficiency in a fully copper-metallized HJT cell, with a relatively small efficiency penalty compared with a silver-metallized counterpart. Cells combining silver-copper paste on the front side with silver contacts on the rear reached 23.95%. Those results point to copper’s potential for reducing silver use, while further improvements in processing and electrical performance are still needed.